| Fluorocarbon solvent Hydrochlorofluorocarbon (Chlorodifluoromethane, Freon 22) | ||||
| Chemical formula: CHClF2 | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density of gas at at boiling point | 4.71 | kg/m³ | 0.29 | lb/ft³ | 
|---|---|---|---|---|
| Density of liquid at boiling point | 1.413*10³ | kg/m³ | 88.2 | lb/ft³ | 
| Viscosity at 32°F (0°C) | 0.126 | cP | 8.47*10-5 | lb/ft·s | 
| Vapor pressure at 68°F (20°C) | 908 | kPa | 132 | psi | 
| Boiling point | -41 | ºC | -41 | ºF | 
| Melting point | -175 | ºC | -284 | ºF | 
| Specific heat capacity (Cv) of gas at 86°F (30°C) | 555 | J/(kg*K) | 0.133 | BTU/(lb*ºF) | 
| Specific heat capacity (Cp) of gas at 86°F (30°C) | 659 | J/(kg*K) | 0.157 | BTU/(lb*ºF) | 
| Latent heat of vaporization | 234 | kJ/kg | 101 | BTU/lb |