to Spinodal Bronzes
to Properties of copper alloys
(submitted by the website administration)
| Spinodal Bronze Nicomet | ||||
| Chemical composition: Ni=5.75%, Sn=5.75%, Zn=1.75%, Cu=balance | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 8.86 *10³ | kg/m³ | 553 | lb/ft³ |
|---|---|---|---|---|
| Thermal conductivity | 53.7 | W/(m*K) | 372 | BTU*in/(hr*ft²*ºF) |
| Electric conductivity | 12% | I.A.C.S. | 12% | I.A.C.S. |
| Tensile strength | 517 | MPa | 75000 | psi |
| Yield strength | 345 | MPa | 50000 | psi |
| Elongation | 5 | % | 5 | % |
| Hardness | 90 | RB | 90 | RB |